KX Alloy 40 Corrosion Resistant Alloy Light Rod On Expansion Alloy

Categories Expansion Alloy
Brand Name: KAIXIN
Model Number: KX-Alloy40
Certification: ISO9001:2015
Place of Origin: China
MOQ: 200KG
Price: To negotiate
Payment Terms: T/T, L/C
Supply Ability: 50~80TONS per MONTH
Delivery Time: 45~60days
Packaging Details: Wooden Box, size as per guests's request
Shape: Wire,Strip,Rod,Tube,Plate
Alloy Type: Iron Nickel Cobalt Alloy
Raw Materials: NI32.4-33.4%,CO7-8%,Fe Rem
Executive standard: YB/T 5241
Delivery State: Soft State
Application: To produce a variety of klystron, microwave tube cavity in the electric vacuum industry
Features: Low linear expansion coefficient in the range of 20-100°C and easy to cut machining.
Size: Negotiable
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
Submit Buying Request
  • Product Details
  • Company Profile

KX Alloy 40 Corrosion Resistant Alloy Light Rod On Expansion Alloy

Product Description and Application

Alloy 40 is also known as 4J40

Alloy 40 is Fe-Ni-Co ternary alloy and its curie point is above 300℃. The alloy has a low expansion coefficient in the temperature range of -20 ~ 300℃, and the transformation from austenite (γ) to martensite (M) does not occur until -60℃. The alloy is mainly used in the manufacture of highly precise instrument parts and electronic devices requiring sizes in the temperature range of -50 to 300℃


Process Performance and Requirements


  • Product Fusion Process

Vacuum Induction Furnace(VIM) and Electroslag Remelting Furnace(ESR)


  • Product Chemical Composition

Alloy GradeChemical Composition (mass fraction)(%)
CSiPSMnCuNiCoFe
Alloy 400.050.150.020.020.25---32.4~33.47.0~8.0Rem

  • Product Linear Expansion Coefficient

Alloy GradeSample Heat Treatment InstitutionAverage coefficient of linear expansionα(10-6/ K)
20~100℃20~300°C
4J40The semi-finished sample was heated to 840±10°C, hold for 1 hour, water quenched, and then the sample was processed into finished sample. Heat preservation 1 hour at 315±l0℃ with furnace cooling or air cooling≤2.0

  • Product Typical Average Linear Expansion Coefficient

Alloy Grade

Average Coefficient of Linear Expansion

α(10-6/ K)

20~50℃20~100℃20~200℃20~300℃20~400℃20~500℃
4J401.41.31.21.74.5

  • Productive Process


  • Professional Customization

Cold-drawn Wire¢0.3~¢18mm(Delivery in rolls or trays)
Hot-Rolling Wire¢5.5~¢20mm(Delivery in rolls)
Stripthickness 0.1~4.5*width 6~350mm(Supply in rolls or straight strips)
Smooth Forged Rod on a Lathe

¢60~350mm,L800-2500mm

Hot-rolled Burnishing¢20~80mm,L1000-5000mm
Cold Drawn and Burnishing¢2.5~18mm,L1000-8000mm
Seamless Tube¢1~275mm,wall thickness 0.2~30,L1000-8000mm

Quality KX Alloy 40 Corrosion Resistant Alloy Light Rod On Expansion Alloy for sale
Send your message to this supplier
 
*From:
*To: Danyang Kaixin Alloy Material Co., Ltd.
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0